不用返工的腻子粉施工工艺!

来源:https://www.jnfhjc.com 日期:2019-07-25 发布人:

  家庭装修时,一般都会选择腻子粉,那么如何掌握腻子粉施工的工艺呢?这样以后就不用返工了,下面小编为您做一下腻子粉制作的重点介绍:

  Family decoration, the general choice of putty powder, then how to master the putty powder construction process? In this way, there is no need to rework later, the following Xiaobian for you to do the focus of putty powder production:
  施工准备:
  Construction preparation:
  1. 防水腻子膏材料检查:每批防水腻子进入现场后,随机选择3袋进行施工检查,检查设置时间、细度、白度及与基层的粘结强度。不合格的不得使用。
  1. Inspection of waterproof putty paste materials: After each batch of waterproof putty enters the site, three bags are randomly selected for construction inspection, and the setting time, fineness, whiteness and bonding strength with the base are checked. Unqualified must not be used.
  2、工具准备:湿喷锅或辊刷、0.2mm厚的不锈钢刮刀、2把直尺、水平尺、腻子刀1-2英寸、料斗、料斗、粉袋、扫帚、刀、刷、刷、线滴、直尺。
  2. Tool preparation: wet spraying pot or roller brush, 0.2mm thick stainless steel scraper, 2 rulers, horizontal ruler, putty knife 1-2 inches, hopper, hopper, powder bag, broom, knife, brush, line drop, ruler.
  工艺流程:
  Technological process:
  根据产品手册进行治疗→混合防水和油腻的水→刮防水和油腻的首次→厚度不应小于0.8毫米→挂网布和平整墙壁→修复和水准阴阳角和一些水平角→刮防水和油腻的水角的第二次,厚度约0.5毫米→正确的阴阳角→修复棱角→波兰和出版社。
  According to the product manual for treatment mixed waterproof and greasy water scraping waterproof and greasy first thickness should not be less than 0.8mm hanging mesh cloth and flat wall repair and level Yin and Yang angle and some horizontal angle scraping waterproof and greasy water angle second, thickness is about 0.5mm correct Yin and Yang angle repair edge angle Poland And publishing houses.
  1、寻找弹簧线的规律,粘贴防污染胶带。
  1. Search for the law of spring line and stick anti-pollution tape.
  2. 在门窗边缘和装饰线周围粘贴防污染条。
  2. Stick anti-pollution strips around the edges of doors and windows and decorative lines.
  3.混合防水腻子。
  3. Mixed waterproof putty.
  根据厂家提供的使用比例搅拌后即可施工。调质腻子不宜太多,用多少调,用多少调,应在两小时内用完。
  According to the proportion provided by the manufacturer, it can be constructed after mixing. Conditioning putty should not be too much, how many adjustments, how many adjustments, should be used up in two hours.
济南腻子粉
  4、基层处理
  4. Grass-roots treatment
  不同类型、不同厂家的腻子使用不一样,在基本处理时应严格按照厂家的说明进行处理。
  Putties of different types and manufacturers are used differently, and they should be treated strictly according to the manufacturer's instructions in the basic treatment.
  5、一般一层腻子用两次才能存活
  5. A layer of putty can survive only twice.
  腻子厚度0.5 ~ 1.5mm。次刮腻子时要找平时,腻子厚度0.5 ~ 0.8mm至均匀成型。腻子厚度约0.3 ~ 0.5mm。工艺以水平和垂直、力向均匀、覆盖油脂达到匀光、不突然变轻和变重,以避免不同颜色、糊现象。表面腻子应在腻子固化前完成。第二层表面腻子不留痕迹,大面积表面光滑,光线方向自然,适合采光。腻子次与第二次之间的间隔时间和压光时间应根据具体产品确定,并应服从制造商的指示。
  Putty thickness is 0.5-1.5 mm. When scraping putty for the first time, the thickness of putty should be from 0.5 mm to 0.8 mm until it is evenly shaped. Putty thickness is about 0.3-0.5 mm. In order to avoid different color and paste phenomena, the technology uses horizontal and vertical, uniform force direction, uniform coverage of grease, no sudden lightening and weight change. Surface putty should be finished before putty curing. The second layer of putty does not leave traces, large area of smooth surface, natural light direction, suitable for lighting. The interval and calendering time between the first and the second time of putty shall be determined according to the specific product and shall be subject to the instructions of the manufacturer.
  6、腻子要刮实轻压实
  6. Putty should be scraped and compacted
  刮擦均匀,效果光滑,对于划痕和不平,宜采用40 ~ 60目砂纸研磨。作为后的装饰层的腻子,如油漆在这个表面,应用水砂纸到哑光表面。
  Scraping is even and the effect is smooth. For scratches and unevenness, 40 - 60 mesh sandpaper is suitable for grinding. Putty as the final decorative layer, such as paint on this surface, apply sandpaper to matte surface.
  7. 打磨和抛光
  7. Grinding and Polishing
  第二次刮腻子后应及时除去装饰线的橡胶条,清洗并修补边角,用腻子刀挖洞,阴阳角,装饰线多余的腻子铲铲,清洗干净,达到线条清晰,无污染。凹面修补应先将水辊打湿,刮削修补处略高于原墙面,待完全干燥后,用细砂纸磨平抹平。
  After scraping putty for the second time, the rubber strips of decorative lines should be removed in time, the edges and corners should be cleaned and repaired, the holes should be digged with putty knife, the Yin and Yang angles should be used, and the excess putty shovels and shovels of decorative lines should be cleaned, so that the lines are clear and pollution-free. Concave repair should first wet the water roller, scraping repair slightly higher than the original wall, to be completely dry, with fine sandpaper grinding flat.