腻子在批刮过程中比较沉是怎么回事?

来源:https://www.jnfhjc.com 日期:2021-10-19 发布人:

在这种情况下,纤维素的粘度通常太高。有的厂家使用粘度为20万的纤维素来制作腻子。由于腻子粘度大,刮腻子时显得厚重,内壁腻子一般。推荐用量3~5公斤,粘度8万~10万。

In this case, the viscosity of cellulose is usually too high. Some manufacturers use cellulose with viscosity of 200000 to make putty. Due to the high viscosity of putty, it appears thick when puttying, and the putty on the inner wall is general. The recommended dosage is 3 ~ 5kg and the viscosity is 80000 ~ 100000.
防水腻子很难打磨?
Waterproof putty is difficult to polish?
由于耐水腻子强度高,产品附着力大,腻子粉厂家,比不耐水腻子更难搅拌和刮擦。耐水腻子的强度也比不耐水腻子高,打磨会比较费力。
Due to the high strength of water-resistant putty and high product adhesion, putty powder manufacturers are more difficult to stir and scrape than water-resistant putty. The strength of water-resistant putty is also higher than that of non water-resistant putty, and grinding will be more laborious.
1、施工时尽量不要留下划痕。如果有划痕,可以用工具刮掉。
1. Try not to leave scratches during construction. If there are scratches, they can be scraped off with a tool.
2、腻子层90%干后再安排打磨,省力又不粘砂纸。
2. Polishing shall be arranged after 90% of the putty layer is dry, which saves labor and does not stick sandpaper.
3、抛光后应立即清除表面灰尘层,内外墙腻子粉,防止二次室内灰尘污染。
3. After polishing, the dust layer on the surface and putty powder on the inner and outer walls shall be removed immediately to prevent secondary indoor dust pollution.
4、手工打磨时,将砂纸(布)包在打磨垫上,用力推动打磨垫。不能只用一两根手指按压砂纸进行打磨,以免影响打磨的平整度。对于机械抛光,通常使用电动研磨机。砂纸夹在研磨机上,轻轻推在基层上。严禁用力按压,以免电机过载损坏。
4. During manual grinding, wrap sandpaper (cloth) on the grinding pad and push the grinding pad hard. Do not use one or two fingers to press the sandpaper for grinding, so as not to affect the flatness of grinding. For mechanical polishing, an electric grinder is usually used. The sandpaper is clamped on the grinder and gently pushed on the base course. Do not press hard to avoid motor overload damage.
腻子粉刮的时候明显很重。腻子粉是腻子粉主要选用纤维素。腻子粉可以保证施工时的和易性,内外墙腻子粉厂家,不会造成脱粉等问题。有直接关系。
The putty powder is obviously heavy when scraping. Putty powder is mainly cellulose. Putty powder can ensure the workability during construction. The manufacturer of putty powder for internal and external walls will not cause problems such as powder removal. Directly related.